Fuel rod welding (LWBR development program)
Description
Procedures were developed to weld both ends of approximately 25,000 fuel rods for the Light Water Breeder Reactor (LWBR) core. The rods were welded using the gas tungsten arc (GTA) method in high-purity helium at 1 atmosphere. Welding parameters, including weld current, arc gap, and speed of rotation, were established to control the size of the weld. Electrode and chill positioning with respect to the endclosure/tube joint controlled the location of the weld. Weld quality of the fuel rods was ensured by 100-percent nondestructive testing by ultrasonic and radiographic inspection and the destructive evaluation of process control samples in each weld lot
Availability note (English)
MF available from INIS under the Report Number; Available from NTIS., PC A04/MF A01.
Files
Additional details
Publishing Information
- Imprint Pagination
- 54 p.
- Report number
- WAPD-TM--1235
INIS
- Country of Publication
- United States
- Country of Input or Organization
- United States
- INIS RN
- 10473949
- Subject category
- S21: SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS;
- Descriptors DEI
- FUEL CANS; FUEL RODS; INSPECTION; LWBR TYPE REACTORS; PERFORMANCE; QUALITY CONTROL; REACTOR CORES; WELDED JOINTS; WELDING; ZIRCALOY 4
- Descriptors DEC
- ALLOYS; BREEDER REACTORS; CONTROL; FABRICATION; FUEL ELEMENTS; JOINING; JOINTS; REACTOR COMPONENTS; REACTORS; THERMAL REACTORS; TIN ALLOYS; TRANSITION ELEMENT ALLOYS; WATER COOLED REACTORS; WATER MODERATED REACTORS; ZIRCALOY; ZIRCONIUM ALLOYS; ZIRCONIUM BASE ALLOYS