Published August 1987 | Version v1
Journal article

Statistics applied to the testing of cladding tubes

Creators

  • 1. Cogema, Grenoble (France)

Description

Cladding tubes, either steel or zircaloy, are generally given a 100 % inspection through ultrasonic non-destructive testing. This inspection may be completed beneficially with an eddy current test, as this is not sensitive to the same defects as those typically traced by ultrasonic testing. Unfortunately, the two methods (as with other non-destructive tests) exhibit poor precision; this means that a flaw, whose size is close to that denoted as rejection limit, may be accepted or rejected. Currently, rejection, i.e. the measurement above which a tube is rejected, is generally determined through measuring a calibration tube at regular time intervals, and the signal of a given tube is compared to that of the most recently completed calibration. This measurement is thus subject to variations which can be attributed to an actual shift of adjustments as well as to poor precision. For this reason, monitoring instrument adjustments using the so-called control chart method are proposed

Additional details

Publishing Information

Journal Title
Nucl. Eur.
Journal Volume
7
Journal Issue
8-9
Series
Nucl. Eur.
Journal Page Range
20
ISSN
0254-8348
CODEN
NUEUD

INIS

Country of Publication
Switzerland
Country of Input or Organization
Switzerland
INIS RN
18100192
Subject category
S42: ENGINEERING;
Descriptors DEI
FUEL CANS; INSPECTION; NONDESTRUCTIVE TESTING; STATISTICS
Descriptors DEC
MATERIALS TESTING; MATHEMATICS; TESTING