The dielectric constant of UO2 below the Neel point
- 1. Bath Univ. (UK). School of Physics
- 2. UKAEA Atomic Energy Research Establishment, Harwell. Theoretical Physics Div.
Description
We report measurements of the frequency-dependent dielectric constant of UO2 from 4.2 K to above the phase transition at 30 K. The static dielectric constant of 23.6 at 4.2 K is comparable with accepted values at higher temperatures: it is essentially identical in both phases. The effects of undergoing the transition on the dielectric constant are marginal (about 1%) and take place in the temperature range 29 K to 37 K. The displacement of the oxygen sublattice, which occurs at the Neel point, should produce only a 0.05% change on the dielectric constant and of the opposite sense to that measured. Hence the structural changes at the transition are not the primary source of the observed small difference between the dielectric constant in the two phases which probably accrues from the influence of the displacement on a defect-related contribution. (orig.)
Additional details
Publishing Information
- Journal Title
- J. Nucl. Mater.
- Journal Volume
- 149
- Journal Issue
- 1
- Series
- J. Nucl. Mater.
- Journal Page Range
- 18-20
- ISSN
- 0022-3115
- CODEN
- JNUMA
INIS
- Country of Publication
- Netherlands
- Country of Input or Organization
- Netherlands
- INIS RN
- 18089029
- Subject category
- S36: MATERIALS SCIENCE;
- Resource subtype / Literary indicator
- Numerical Data
- Descriptors DEI
- CAPACITANCE; EXPERIMENTAL DATA; FREQUENCY DEPENDENCE; NEEL TEMPERATURE; PERMITTIVITY; PHASE TRANSFORMATIONS; TEMPERATURE DEPENDENCE; ULTRALOW TEMPERATURE; URANIUM DIOXIDE; VERY LOW TEMPERATURE
- Descriptors DEC
- ACTINIDE COMPOUNDS; CHALCOGENIDES; DATA; DIELECTRIC PROPERTIES; ELECTRICAL PROPERTIES; INFORMATION; NUMERICAL DATA; OXIDES; OXYGEN COMPOUNDS; PHYSICAL PROPERTIES; THERMODYNAMIC PROPERTIES; TRANSITION TEMPERATURE; URANIUM COMPOUNDS; URANIUM OXIDES