Published June 1989
| Version v1
Journal article
Indentation fracture toughness of sintered silicon carbide in the Palmqvist crack regime
Creators
- 1. Argonne National Lab., IL (United States)
- 2. Oak Ridge National Lab., High Temperature Materials Lab., Oak Ridge, TN (United States)
- 3. Washington Univ., Seattle, WA (United States). Coll. of Engineering
- 4. Nevada Univ., Reno, NV (United States). Mackay School of Mines
Description
This paper reports on the fracture toughness of a sintered dense α-SIC estimated by the Vickers indentation microfracture method in the low-load Palmqvist crack regime. It was observed that the use of simultaneously Vickers hardnesses does not yield reliable fracture toughness values, nor does application of the median-crack -derived equation. It is necessary to utilize a load-independent, crack-free hardness value with this toughness estimation method
Additional details
Publishing Information
- Journal Title
- Journal of the American Ceramic Society
- Journal Volume
- 72
- Journal Issue
- 6
- Series
- J. Am. Ceram. Soc.
- Journal Page Range
- 904-911
- ISSN
- 0002-7820
- CODEN
- JACTA
INIS
- Country of Publication
- United States
- Country of Input or Organization
- United States
- INIS RN
- 23018777
- Subject category
- S36: MATERIALS SCIENCE;
- Descriptors DEI
- FRACTURE PROPERTIES; SILICON CARBIDES; SINTERING; VICKERS HARDNESS
- Descriptors DEC
- CARBIDES; CARBON COMPOUNDS; FABRICATION; MECHANICAL PROPERTIES; SILICON COMPOUNDS