Published July 2007 | Version v1
Journal article

Residual stress in zirconia coating by EB-PVD method

  • 1. Niigata Univ., Dept. of Technology and Living Science, Niigata (Japan)
  • 2. Toshiba Corp., Power and Industrial Systems Research and Development Center, Yokohama, Kanagawa (Japan)
  • 3. Japan Fine Ceramics Center, Nagoya, Aichi (Japan)
  • 4. Japan Atomic Energy Agency, Quantum Beam Science Directorate, Sayo, Hyogo (Japan)
  • 5. Kawasaki Heavy Industries, Ltd., Technical Inst., Akashi, Hyogo (Japan)
  • 6. Nagoya Univ., Dept. of Mechnical Science and Engineering, Nagoya, Aichi (Japan)

Description

The Ni-based superalloy IN738LC was used as the substrate material, and CoNiCrAlY powder was pressureless plasma-sprayed on the substrate as the bond coating. Zirconia was coated as the top coating by the electron beam-physical vapor deposition (EB-PVD) method. In the EB-PVD process, the specimens were kept at 1223 K and rotated with 5rpm, 10rpm and 20rpm. According to the microscopic observation and the result of the pole figures, the top coatings had a columnar structure, which was made by the piling up of (111) planes. The cross section of the column had a diamond shape, and its diagonal was parallel to the rotation axis. The residual stress on the surface of the top coatings was evaluated by the X-ray diffraction method. Each diffraction profile was separated into the 133 and the 331 peak, and the residual stress was measured by the sin2 ψ method. The measured residual stresses were -76.7 MPa for 5rpm, -63.0MPa for 10rpm and -25.1MPa for 20rpm. (author)

Additional details

Publishing Information

Journal Title
Zairyo
Journal Volume
56
Journal Issue
7
Journal Page Range
p. 588-593