A fracture mechanics interpretation of acoustic emission results
Creators
- 1. Kernforschungszentrum Karlsruhe G.m.b.H. (Germany, F.R.). Projektbereich Heissdampfreaktor - Sicherheitsprogramm/Handhabungstechnik
- 2. Fraunhofer-Institut fuer Zerstoerungsfreie Pruefverfahren, Saarbruecken (Germany, F.R.)
Description
The observation of crack propagation processes during cyclic thermal shock experiments with a corrosive medium on a clad pressure vessel plange of a superheated steam-cooled reactor was conducted with a sonic emission system with which the sonic emission reflections of the crack propagation and other processes (such as crack friction) could be automatically classified. This classification is conducted on the basis of a statistic model, whereby for each sonic reflection, different signal parameters (rise time, duration and energy of the signal) are taken into consideration. From the sonic test results of the thermal shock-loaded flange experiments, an important new conclusion concerning the crack propagation mechanism seems possible. This is that the crack growth is not primarily dependent on the load delta-K, but only occurs during a short period of unfavourable temperature. These deductions are to be investigated in detail in aimed future experiments. (orig./DG)
Abstract (German)
Zur Ueberwachung von Rissausbreitungsvorgaengen bei zyklischen Thermoschock-Experimenten mit korrosivem Medium an einem plattierten Druckbehaelterstutzen des HDR wurde ein Schallemissionssystem eingesetzt, mit dem Schallemissionsereignisse nach Rissfortschritt und anderen Prozessen (wie Rissreibung) automatisch klassifiziert werden. Die Einstufung erfolgt auf Basis eines statistischen Modells, wobei pro Schallemissionsereignis verschiedene Signalparameter (Anstiegszeit, Dauer und Energie des Signals) beruecksichtigt werden. Das Schallemissionsergebnis legt als wichtige neue Schlussfolgerung zum Mechanismus des Risswachstums im konkreten Fall der Thermoschock-Stutzenexperimente nahe, dass das Risswachstum nicht primaer von der Last Delta-K abhaengt, sondern nur in einer kurzen Zeitspanne unguenstiger Temperatur erfolgt. Diese Schlussfolgerungen sollen bei der Fortsetzung der Untersuchungen am HDR-RDB gezielt ueberprueft werden. (orig./DG)Additional details
Additional titles
- Original title (German)
- Werkstoffmechanische Interpretation von Ergebnissen der Schallemissionspruefung
Publishing Information
- Imprint Title
- Safety and reliability of pressure components with special emphasis on the contribution of component and large specimen testing to structural integrity assessment methodology. Vol. 1 and 2
- Imprint Pagination
- 1129 p.
- Journal Page Range
- p. 26.1-26.26.
- Report number
- INIS-mf--11982
Conference
- Title
- The contribution of component and large specimen testing to structural integrity assessment methodology.
- Original Conference Title
- 13. MPA Seminar ueber Sicherheit und Verfuegbarkeit in der Anlagentechnik: Der Beitrag der Komponenten- und Grossprobenpruefung zur Beurteilung von Bauteilen und Anlagen
- Acronym
- 13. MPA seminar on safety and reliability of pressure components
- Dates
- 8-9 Oct 1987.
- Place
- Stuttgart (Germany, F.R.).
INIS
- Country of Publication
- Germany
- Country of Input or Organization
- Germany
- INIS RN
- 20057104
- Subject category
- S42: ENGINEERING; S22: GENERAL STUDIES OF NUCLEAR REACTORS;
- Resource subtype / Literary indicator
- Conference
- Descriptors DEI
- ACOUSTIC EMISSION TESTING; CRACK PROPAGATION; FLANGES; FRACTURE MECHANICS; PRESSURE VESSELS; REACTOR SAFETY EXPERIMENTS; VALVES
- Descriptors DEC
- ACOUSTIC TESTING; CONTAINERS; CONTROL EQUIPMENT; EQUIPMENT; FLOW REGULATORS; MATERIALS TESTING; MECHANICS; NONDESTRUCTIVE TESTING; TESTING
Optional Information
- Notes
- Imprint:Published in 2 separate volumes.;Sicherheit und Verfuegbarkeit in der Anlagentechnik mit dem Schwerpunkt 'Der Beitrag der Komponenten- und Grossprobenpruefung zur Beurteilung von Bauteilen und Anlagen'. Bd. 1 und 2.;Bd. 1: Bruchmechanik, dynamische Beanspruchung, zerstoerungsfreie Pruefungen, strahleninduzierte Versproedung. Bd. 2: Rohrleitungsversagen, Komponenten, Thermoschock, Hochtemperaturverhalten, Behaelterintegritaet, Schweissverbindungen.