Corrosion behavior of Nd9.4Pr0.6Febal.Co6B6Ga0.5TixCx (x=0, 1.5, 3, 6) nanocomposites annealed melt-spun ribbons

  • 1. School of Metallurgy and Materials Engineering, Faculty of Engineering, University of Tehran, Tehran 11155-4563 (Iran, Islamic Republic of)
  • 2. Iranian Research Organization for Science and Technology (IROST), Tehran 15815-3538 (Iran, Islamic Republic of)
  • 3. National Institute for Materials Science, 1-2-1 Sengen, Tsukuba 305-0047 (Japan)

Description

The effect of Ti and C additions on the corrosion behavior of Nd9.4Pr0.6Febal.Co6B6Ga0.5TixCx (x=0, 1.5, 3, 6) isotropic nanocomposite melt-spun ribbons in 3.5 wt% sodium chloride solution was studied. The melt-spun ribbons were annealed at 750 oC for 10 min in argon-filled quartz capsules. The microstructure of multiphase nanocrystalline samples and corrosion products was characterized using the X-ray diffraction and electron microscopy techniques. The electrochemical behavior was assessed using potentiodynamic polarization and electrochemical impedance spectroscopy. The results show that the addition of Ti and C increases the corrosion resistance of NdFeB ribbons; the best corrosion resistance was obtained for 1.5 wt% Ti and C content.

Availability note (English)

Available from http://dx.doi.org/10.1016/j.jmmm.2009.06.053

Additional details

Identifiers

DOI
10.1016/j.jmmm.2009.06.053;
PII
S0304-8853(09)00646-5;

Publishing Information

Journal Title
Journal of Magnetism and Magnetic Materials
Journal Volume
321
Journal Issue
20
Journal Page Range
p. 3391-3395
ISSN
0304-8853
CODEN
JMMMDC

Optional Information

Copyright
Copyright (c) 2009 Elsevier Science B.V., Amsterdam, The Netherlands, All rights reserved.