Fundamental weld metallurgical investigations on laser beam welding of non- and micro alloyed steels. Final report

Description

During Laser beam welding of structural steels with plate thickness above 10 mm solidification cracks and lower toughness occur. Aim of that project was to determine the process parameters, which allow the Laser beam welding without lower toughness values. Furthermore different alloying elements should be investigated regarding its influence of solidification cracking and toughness. (orig.)

Availability note (English)

Available from INIS in electronic form

Abstract (German)

Beim Laserstrahlschweissen von Baustaehlen im Blechdickenbereich oberhalb 10 mm treten Heissrisse und ein Zaehigkeitsabfall im Bereich der Schweissnaht auf. Ziel der durchgefuehrten Untersuchungen war die Prozessparameter zu ermitteln, die eine rissfreie Schweissung ohne Zaehigkeitsabfall ermoeglichen. Ausserdem sollten die Einfluesse unterschiedlicher Legierungselemente auf die Heissrissbildung und Zaehigkeit untersucht werden. (orig.)

Files

Restricted

The record is publicly accessible, but files are restricted to users with access.

Additional details

Additional titles

Original title (German)
Anforderungsangepasste Schweisszusatzwerkstoffe zum Laserstrahlschweissen. Grundlegende schweissmetallurgische Untersuchung beim Laserstrahlschweissen un- und mikrolegierter Staehle. Abschlussbericht

Publishing Information

Imprint Pagination
25 p.
Report number
INIS-DE--0057

INIS

Optional Information