Published February 2, 2000 | Version v1
Report Open

Estimating model parameter values for total system performance assessment

Description

The intrinsic dissolution rates of nine borosilicate waste glasses were extracted from the results of MCC-1 tests conducted for durations long enough that the solution pH reached a nearly constant value but short enough that the buildup of dissolved species did not affect the dissolution rate. The effects of the pH and temperature on the measured rates were deconvoluted to determine the sensitivity of the rate to the glass composition. The intrinsic dissolution rates were similar for all of these glasses and were not correlated with the glass composition. The mean and standard deviation of the intrinsic dissolution rates of these glasses are log k0/[g/(m2·d)] = 8.2 ± 0.2

Availability note (English)

Available from INIS in electronic form; Also available from OSTI as DE00751836; PURL: https://www.osti.gov/servlets/purl/751836-nJcb4w/webviewable/

Files

31047213.pdf

Files (174.3 kB)

Name Size Download all
md5:bcc71ee29fa9b334a1ec716270282ad6
174.3 kB Preview Download

Additional details

Publishing Information

Imprint Pagination
10 p.
Report number
ANL/CMT/CP--99344

Conference

Title
Materials Research Society Annual Fall Meeting
Dates
29 Nov - 3 Dec 1999
Place
Boston, MA (United States)

Optional Information

Contract/Grant/Project number
W-31109-ENG-38
Funding organization
US Department of Energy (United States)