Irradiation creep and IASCC prediction method of PWR's core internal. Verification of ''Inspection and evaluation guideline for reactor internals of PWR(baffle former bolt)
- 1. The Kansai Electric Power Co., Inc., Osaka (Japan)
- 2. Mitsubishi Heavy Industries, LTD., Tokyo (Japan)
Description
PWR's core internals have aging due to IASCC (Irradiation Assisted Stress Corrosion Cracking). Although stress influences the occurrence of IASCC greatly, we have little data about PWR's irradiation creep which reduces stress. In this report, we assessed irradiation creep by using the removal torque of the baffle former bolts at the time of replacement. Then, we concluded that irradiation creep in PWR is approximately 50% of the irradiation creep in the fast breeder reactor. Moreover, we used this result to check the method for IASCC prediction method proposed in the last report which is applicable also to barrel former bolt and weld metal of barrel, and we confirmed the applicability of the IASCC prediction method for the actual plant. (author)
Additional details
Publishing Information
- Journal Title
- Yosetsu Gakkai Ronbunshu
- Journal Volume
- 23
- Journal Issue
- 1
- Journal Page Range
- p. 77-81
- ISSN
- 0288-4771
INIS
- Country of Publication
- Japan
- Country of Input or Organization
- Japan
- INIS RN
- 36053695
- Subject category
- S21: SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS;
- Descriptors DEI
- CRACKS; CREEP; EVALUATION; FASTENERS; INSPECTION; IRRADIATION; PWR TYPE REACTORS; REACTOR VESSELS; STRESS CORROSION; VERIFICATION
- Descriptors DEC
- CHEMICAL REACTIONS; CONTAINERS; CORROSION; ENRICHED URANIUM REACTORS; MECHANICAL PROPERTIES; POWER REACTORS; REACTORS; THERMAL REACTORS; WATER COOLED REACTORS; WATER MODERATED REACTORS
Optional Information
- Notes
- 5 refs., 9 figs.