Process for producing formed parts containing high-activity waste and consisting of glass granules in a metal matrix

Description

Glass balls are mixed with lead powder until a macroscopically homogeneous distribution of the two powders in the suspension is achieved. Then the mixing fluid is evaporated, the mixture is pressed into steel matrices and resintered. (orig./PW)

Availability note (English)

MF available from INIS under the Report Number.

Files

17074091.pdf

Files (143.7 kB)

Name Size Download all
md5:bddbceae9a986c78661371455f8b6315
143.7 kB Preview Download

Additional details

Additional titles

Original title (German)
Verfahren zur Verfestigung hochradioaktiver Abfallstoffe enthaltender, als Granalien oder als Pulver vorliegender Glasteilchen in einer Metallmatrix