Pelleted waste form for high-level ICPP wastes

Description

Simulated zirconia type calcined waste is pelletized on a 41-cm dia disc pelletizer using 5% bentonite, 2% metakaolin, and 2% boric acid as a solid binder and 7M phosphoric plus 4M nitric acid as a liquid binder. After heat treatment at 8000C for 2 hours, the pellets are impact resistant and have a leach resistance of 10-4 g/cm2/day, based on Soxhlet leaching for 100 hours at 950C with distilled water. An integrated pilot plant is being fabricated to verify the process. 1 figure, 4 tables

Availability note (English)

MF available from INIS under the Report Number; Available from NTIS., PC A02/MF A01.

Files

10474205.pdf

Files (259.3 kB)

Name Size Download all
md5:001ed2a6b890274d5deb0e3c42b2a618
259.3 kB Preview Download

Additional details

Publishing Information

Imprint Pagination
17 p.
Report number
CONF-790420--2

Conference

Title
International symposium on ceramics in nuclear waste management.
Dates
30 Apr - 2 May 1979.
Place
Cincinnati, OH, USA.