Fracture Analysis of Cast Steel Sling
Creators
- 1. Department of Architecturl Engineering,Jiangsu Prvince Xuzhou Technician Institute Xuzhou, Jiangsu (China)
Description
The fracture reasons of ZG270-500 cast steel sling are analyzed through such means as macroscopic morphology analysis, chemical composition analysis, and microscopic metallography analysis. Results: coarse Widmanstatten structure and casting defects occurring in casting and subsequent heat treatment process reduce the strength, plasticity and toughness of the steel, which is the main reason of brittle fracture of the sling during work, and corresponding improvement suggestions are proposed herein. (paper)
Availability note (English)
Available from http://dx.doi.org/10.1088/1757-899X/307/1/012071Additional details
Identifiers
Publishing Information
- Journal Title
- IOP Conference Series. Materials Science and Engineering (Online)
- Journal Volume
- 307
- Journal Issue
- 1
- Journal Page Range
- [4 p.]
- ISSN
- 1757-899X
Conference
- Title
- International Conference on Mechanical Engineering and Applied Composite Materials
- Dates
- 23-24 Nov 2017
- Place
- Hong Kong (China)
INIS
- Country of Publication
- United Kingdom
- Country of Input or Organization
- International Atomic Energy Agency (IAEA)
- INIS RN
- 52072637
- Subject category
- S36: MATERIALS SCIENCE;
- Resource subtype / Literary indicator
- Conference
- Descriptors DEI
- CASTING; CASTINGS; CHEMICAL COMPOSITION; DEFECTS; FRACTURES; HEAT TREATMENTS; METALLOGRAPHY; MORPHOLOGY; PLASTICITY; STEELS; WIDMANSTAETTEN STRUCTURE
- Descriptors DEC
- ALLOYS; CARBON ADDITIONS; FABRICATION; FAILURES; IRON ALLOYS; IRON BASE ALLOYS; MECHANICAL PROPERTIES; MICROSTRUCTURE; TRANSITION ELEMENT ALLOYS