On the optimisation of etching conditions for CR-39 and other plastic track detectors

Description

Selection of optimum etching conditions for plastic track detectors is essential if they are to be used to best advantage. Results are presented of a study of the influence of etchant type, temperature and concentration, on the etching response of CR39. It is concluded that 6N NaOH at 700C gives the steepest response curve for CR39, within the range of temperatures (40 to 700C) and concentrations (1N to 12N) studied. Other plastics are briefly discussed. (author)

Additional details

Publishing Information

Publisher
Pergamon.
Imprint Place
Oxford
ISBN
0-08-026509-X
Imprint Title
Solid state nuclear track detectors
Imprint Pagination
958 p.
Journal Page Range
p. 179-182.

Conference

Title
11. international conference on solid state nuclear track detectors.
Dates
7 - 12 Sep 1981.
Place
Bristol, UK.

Optional Information

Notes
Imprint:Supplement 3. to nuclear tracks, methods, instruments and applications.