Published September 1982 | Version v1
Report

Creep deformation and crack growth in a low alloy steel welded pressure vessel containing defects

Creators

  • 1. Central Electricity Generating Board, Southampton, England

Description

A full-size pressure vessel was tested for effects of welding residual stresses on creep deformation and crack growth. The vessel, based on 1/2 Cr 1/2 Mo 1/4 V main steam pipe, contained four 2CrMo manual metal arc welds, two in the as-welded condition and two stress-relieved. All the welds contained pre-existing defects machined in the heat affected zones. Testing was carried out at two internal steam pressures, 250 and 350 bar, and 5650C. Cracked and uncracked areas of the vessel were monitored continuously. Results are presented for the continuous creep deformation observed in both the hoop and axial directions of the welds throughout the 11,400 h of testing, as well as the intermittent strain data obtained during inspections. Crack growth observations are described based on nondestructive examination. The residual stresses measured are also given for both the as-welded and stress relieved weldments. Results obtained are discussed in terms of the effects of welding residual stress on the hoop and axial deformations observed in the welds. Similarly, the effects of residual stress on creep crack growth are considered together with compositional and microstructural implications. 9 figures, 5 tables

Additional details

Publishing Information

Imprint Title
Welding technology for energy applications
Journal Page Range
p. 255-277.
Report number
CONF-820544--

Conference

Title
International conference on welding technology for energy applications.
Dates
16 - 19 May 1982.
Place
Gatlinburg, TN (USA).

Optional Information

Notes
Imprint:Portions are illegible in microfiche products.