Published February 1973
| Version v1
Journal article
Kinetic deformation criterions of cyclic destruction at high temperatures
Description
A strain range partitioning method for the analysis of failure by the interaction of creep and fatigue is proposed. A conception is made of the onesided deformation (mean strain) to account for part of the creep damage; the time (and temperature) dependent behavior of the strain to failure is used to modify the common low-temperature low-cycle fatigue equations. Data from 18Cr, 8Ni stainless steel are used as a basis for demonstrating the method. A conventional linear damage summation technique is used for comparison with the results of the proposed method.
Additional details
Additional titles
- Original title (Russian)
- Кинетические деформационные критерии циклического разрушения при высоких температурах
Identifiers
- DOI
- 10.1520/stp38878s;
Publishing Information
- Journal Title
- Fatigue at Elevated Temperatures
- Journal Issue
- no.2
- Series
- Probl. Prochn. Mashinostr.
- Journal Page Range
- 670-677
INIS
- Country of Publication
- USSR
- Country of Input or Organization
- USSR
- INIS RN
- 5102046
- Subject category
- S42: ENGINEERING;
- Descriptors DEI
- CRACKS; CREEP; DEFORMATION; DESTRUCTIVE TESTING; DIAGRAMS; FATIGUE; FRACTURE PROPERTIES; HIGH TEMPERATURE; PLASTICITY; STEEL-KH18N10T; TENSILE PROPERTIES; TIME DEPENDENCE
- Descriptors DEC
- ALLOYS; CHROMIUM ALLOYS; CHROMIUM-NICKEL STEELS; IRON ALLOYS; IRON BASE ALLOYS; MATERIALS TESTING; MECHANICAL PROPERTIES; NICKEL ALLOYS; STAINLESS STEELS; STEELS; TESTING; TITANIUM ADDITIONS; TITANIUM ALLOYS
Optional Information
- Notes
- For English translation see the journal Strength Mater.; Updated automatically by Metadata and Full-Text Enrichment Agent