Published February 28, 2002 | Version v1
Report

B-25 Corrosion Evaluation Summary Report; FINAL

Description

A destructive examination of a B-25 waste storage container that was buried in a shallow non-radiological land burial facility for approximately 8 years showed that pitting was the most prevalent form of corrosion and suggested that continued burial would result in through-wall pits after 30 years. This result suggests that through wall pits will provide a path for water flow into and out of similar B-25 containers after approximately 30 years of burial. Pitting was the most severe on the exterior of the lid. However, the lid had collapsed into the container, probably because the soil loading exceeded the support capacity of the lid. This observation demonstrates that lid strength is a significant factor when assessing structural integrity of the B-25 containers. The lid had collapse had allowed the container to fill with soil and water. A review of procurement specifications for the B-25 containers suggest that the container examined in this work was purchased from an earlier ve rsion of the B-25 container procurement specification

Availability note (English)

Available from www.osti.gov/servlets/purl/799678-EmqTJX/native/

Additional details

Publishing Information

Imprint Pagination
[vp.]
Report number
WSRC-TR--2001-00587

INIS

Country of Publication
United States
Country of Input or Organization
United States
INIS RN
33067291
Subject category
S54: ENVIRONMENTAL SCIENCES;
Resource subtype / Literary indicator
Non-conventional Literature
Descriptors DEI
CAPACITY; CONTAINERS; CORROSION; EVALUATION; PROCUREMENT; SAVANNAH RIVER PLANT; SOILS; SPECIFICATIONS; WASTE STORAGE; WATER
Descriptors DEC
BUSINESS; CHEMICAL REACTIONS; HYDROGEN COMPOUNDS; MANAGEMENT; NATIONAL ORGANIZATIONS; OXYGEN COMPOUNDS; STORAGE; US AEC; US DOE; US ERDA; US ORGANIZATIONS; WASTE MANAGEMENT

Optional Information

Contract/Grant/Project number
AC09-96SR18500
Funding organization
US Department of Energy (United States)