Published April 1983 | Version v1
Journal article

Effect of technological procedures on the crack resistance of nickel alloy welded joints under heat treatment

Description

Comparison of the efficiency of some technological procedures directed to the increase of crack resistance of KhN50MBKTYUR (EhP99) alloy welded joints under heat treatment was conducted. Welded joints were manufactured by the methods of electron beam welding, laser welding, automatic argon-arc welding. The latter was conducted by conventional technology as well as with electromagnetic mixing of liquid metal of welding bath, with compulsory cooling of weld matal, with pulse arc. It is shown that the high fracture resistance of welded joints, manufactured by electron beam and laser welding is achieved by combination of high mechanical properties of heat affected zone metal and reduced elastic potential energy margin of residual welding stresses (as compared to argon-arc welding)

Additional details

Additional titles

Original title (Russian)
Влияние технологических приемов на стойкост' сварных соединений никелевых сплавов против образования трещин при термической обработке

Publishing Information

Journal Title
Svar. Proizvod.
Journal Issue
no.4
Series
Svar. Proizvod.
ISSN
0491-6441

Optional Information

Notes
For English translation see the journal Welding Production (UK).