The grain size of as-cast Ti-6Al-4V is reduced by about an order of magnitude from 1700 to 200 μm with an addition of 0.1 wt.% boron. A much weaker dependence of reduction in grain size is obtained for boron additions from >0.1% to 1.0%. Similar trends were observed in boron-modified as-cast Ti-6Al-2Sn-4Zr-2Mo-0.1Si
Additional details
Identifiers
- DOI
- 10.1016/j.scriptamat.2005.08.020;
- PII
- S1359-6462(05)00503-8;
Publishing Information
- Journal Title
- Scripta Materialia
- Journal Volume
- 53
- Journal Issue
- 12
- Journal Page Range
- p. 1421-1426
- ISSN
- 1359-6462
- CODEN
- SCMAF7
INIS
- Country of Publication
- United Kingdom
- Country of Input or Organization
- International Atomic Energy Agency (IAEA)
- INIS RN
- 38057336
- Subject category
- S36: MATERIALS SCIENCE;
- Descriptors DEI
- BORON; BORON ADDITIONS; CASTING; CASTINGS; GRAIN REFINEMENT; GRAIN SIZE; REFINING; TITANIUM ALLOYS
- Descriptors DEC
- ALLOYS; BORON ALLOYS; ELEMENTS; FABRICATION; MICROSTRUCTURE; PROCESSING; SEMIMETALS; SIZE; TRANSITION ELEMENT ALLOYS
Optional Information
- Copyright
- Copyright (c) 2005 Elsevier Science B.V., Amsterdam, The Netherlands, All rights reserved.