Published August 1988 | Version v1
Report Open

Lifetime analysis of the ITER first wall and divertor plates

Description

The performance of the ITER first wall and divertor plate is analyzed using a 1-D life-time code which includes the effects of radiation damage and surface erosion. The materials considered for the first wall are solution annealed and 20% cold-worked Type 316 stainless steel. The materials considered for the divertor plate are H-451 graphite bonded to a Cu-0.5 Be-2 Ni heat sink. The primary conclusion is that it is crucial to include radiation effects for obtaining realistic predictions of performance. 9 refs., 13 figs., 1 tab

Availability note (English)

MF available from INIS under the Report Number; Available from NTIS, PC A02/MF A01 - OSTI; 1 as DE89003939.

Files

20020505.pdf

Files (215.6 kB)

Name Size Download all
md5:860c5e86eba3389c39e1edcf622197cc
215.6 kB Preview Download

Additional details

Publishing Information

Imprint Pagination
7 p.
Report number
CONF-881031--40

Conference

Title
8. topical meeting on technology of fusion energy.
Dates
9-13 Oct 1988.
Place
Salt Lake City, UT (USA).

Optional Information

Notes
Portions of this document are illegible in microfiche products.