Method for welding chromium molybdenum steels

Creators

Description

A process is described for welding chromium-molybdenum steels which consist of: subjecting the steel to normalization by heating to above the transformation temperature and cooling in air; subjecting the steel to a partial temper by heating to a temperature less than a full temper; welding the steel using an appropriate filler metal; subjecting the steel to a full temper by heating to a temperature sufficient to optimize strength, reduce stress, increase ductility and reduce hardness

Availability note (English)

U.S. Commissioner of Patents, Washington, D.C. 20231, USA, $.50.

Additional details

Publishing Information

Imprint Pagination
vp.
IPC:
Int. Cl. C21D 9/50.
IPC
Int. Cl. C21D 9/50.
Patent number
US patent document 4,612,070/A/

INIS

Country of Publication
United States
Country of Input or Organization
United States
INIS RN
18012633
Subject category
S36: MATERIALS SCIENCE;
Resource subtype / Literary indicator
Non-conventional Literature
Descriptors DEI
AIR; CHROMIUM ALLOYS; COOLING; DUCTILITY; FILLER METALS; HARDNESS; HEATING; MOLYBDENUM ALLOYS; OPTIMIZATION; STEELS; STRESS RELAXATION; TEMPERING; TRANSITION TEMPERATURE; WELDING
Descriptors DEC
ALLOYS; CARBON ADDITIONS; FABRICATION; FLUIDS; GASES; HEAT TREATMENTS; IRON ALLOYS; IRON BASE ALLOYS; JOINING; MECHANICAL PROPERTIES; PHYSICAL PROPERTIES; TENSILE PROPERTIES; THERMODYNAMIC PROPERTIES