The standard Gibbs free energy of formation of lithium manganese oxides at the temperatures of (680, 740 and 800) K
Creators
Description
The standard Gibbs free energy of formation of LiMnO2 and LiMn2O4 at the temperatures of (680, 740 and 800) K has been determined with the help of the solid-state galvanic cells involving lithium-β-alumina electrolyte. The equilibrium electrical potentials of cathode containing LixMn2O4 spinel, in the composition ranges 0≤x≤1 and 1≤x≤2, vs. metallic lithium in the reversible intercalation galvanic cell have been calculated. The existence of two-voltage plateaus which appeared during charging and discharging processes in reversible intercalation of lithium into LixMn2O4 spinel, has been discussed
Additional details
Identifiers
- DOI
- 10.1016/j.jct.2004.02.009;
- PII
- S0021961404000503;
Publishing Information
- Journal Title
- Journal of Chemical Thermodynamics
- Journal Volume
- 36
- Journal Issue
- 6
- Journal Page Range
- p. 473-476
- ISSN
- 0021-9614
- CODEN
- JCTDAF
INIS
- Country of Publication
- United Kingdom
- Country of Input or Organization
- International Atomic Energy Agency (IAEA)
- INIS RN
- 35070816
- Subject category
- S37: INORGANIC, ORGANIC, PHYSICAL AND ANALYTICAL CHEMISTRY;
- Descriptors DEI
- ELECTROLYTIC CELLS; FORMATION FREE ENTHALPY; LITHIUM COMPOUNDS; MANGANESE OXIDES; SPINELS; TEMPERATURE RANGE 0400-1000 K
- Descriptors DEC
- ALKALI METAL COMPOUNDS; CHALCOGENIDES; ENERGY; FREE ENTHALPY; MANGANESE COMPOUNDS; MINERALS; OXIDE MINERALS; OXIDES; OXYGEN COMPOUNDS; PHYSICAL PROPERTIES; TEMPERATURE RANGE; THERMODYNAMIC PROPERTIES; TRANSITION ELEMENT COMPOUNDS
Optional Information
- Copyright
- Copyright (c) 2004 Elsevier Science B.V., Amsterdam, The Netherlands, All rights reserved.