Published January 2007 | Version v1
Journal article

Potential controlled flotation of Sarcheshmeh Molybdenite

  • 1. University of Thehran, Department of Mining Engineering, Tehran (Iran, Islamic Republic of)
  • 2. Yazd University, Yazd (Iran, Islamic Republic of)

Description

Molybdenite flotation in the Sarcheshmeh Copper Complex was studied as a function of pulp potential, controlled using two types of sodium sulfide, a mineral origin and a chemical nature. Air and either plant or laboratory nitrogen were used as flotation careers. Potential readings took place in rougher cells, as it was proved to be vital in the molybdenite circuit. Results showed that, at reducing potentials between -525 and -575 mv, the highest molybdenum recovery of 93% and the lowest copper recovery of 4-15% can be achieved. These potentials did not change considerably by adding extra amounts of sodium sulfide. At more oxidizing potentials, i.e. more than -450 mv, copper recovery increases while the recovery of Molybdenite drops

Availability note (English)

Available from Atomic Energy Organization of Iran

Additional details

Publishing Information

Journal Title
Iranian Journal of Science and Technology. Transaction B, Engineering
Journal Volume
3
Journal Issue
no.B4
Journal Page Range
p. 431-440