Description

Optimum solidification for slurry waste, produced during the operation of KRR-1 and 2, with ordinary Portland cement was investigated. Waste form was prepared by changing the ratio of slurry waste/water/cement. Waste forms were evaluated by workability test, compressive strength test, free standing water test, and immersion test. The experimental results showed that the optimum mixing ratio of slurry waste (dry wt)/water/cement(dry wt) was found to be 0.32/0.34/0.34. The effect of the chemical (EDTA complex, low conc.) in water on waste forms was insignificant

Part of:
Proceedings of the Korean Nuclear Society autumn meeting

Additional details

Publishing Information

Publisher
KNS
Imprint Place
Taejon (Korea, Republic of)
Imprint Title
Proceedings of the Korean Nuclear Society autumn meeting
Imprint Pagination
[CD-ROM]
Journal Page Range
[11 p.]

Conference

Title
2001 autumn meeting of the Korean Nuclear Society
Dates
24-26 Oct 2001
Place
Seoul (Korea, Republic of)

Optional Information

Notes
8 refs, 2 figs, 1 tab