Characteristic length scale of the magnon accumulation in Fe3O4/Pt bilayer structures by incoherent thermal excitation

  • 1. Departamento de Física de la Materia Condensada, Universidad de Zaragoza, E-50009 Zaragoza (Spain)
  • 2. Instituto de Nanociencia de Aragón, Universidad de Zaragoza, E-50018 Zaragoza (Spain)
  • 3. Spin Quantum Rectification Project, ERATO, Japan Science and Technology Agency, Sendai 980-8577 (Japan)
  • 4. WPI Advanced Institute for Materials Research, Tohoku University, Sendai 980-8577 (Japan)
  • 5. Instituto de Ciencia de Materiales de Aragón, Universidad de Zaragoza and Consejo Superior de Investigaciones Científicas, 50009 Zaragoza (Spain)
  • 6. Laboratorio de Microscopías avanzadas, Universidad de Zaragoza, 50018 Zaragoza (Spain)

Description

The dependence of Spin Seebeck effect (SSE) with the thickness of the magnetic materials is studied by means of incoherent thermal excitation. The SSE voltage signal in Fe3O4/Pt bilayer structure increases with the magnetic material thickness up to 100 nm, approximately, showing signs of saturation for larger thickness. This dependence is well described in terms of a spin current pumped in the platinum film by the magnon accumulation in the magnetic material. The spin current is generated by a gradient of temperature in the system and detected by the Pt top contact by means of inverse spin Hall effect. Calculations in the frame of the linear response theory adjust with a high degree of accuracy the experimental data, giving a thermal length scale of the magnon accumulation (Λ) of 17 ± 3 nm at 300 K and Λ = 40 ± 10 nm at 70 K.

Additional details

Identifiers

Publishing Information

Journal Title
Applied Physics Letters
Journal Volume
109
Journal Issue
1
Journal Page Range
vp.
ISSN
0003-6951
CODEN
APPLAB

Optional Information

Notes
(c) 2016 Author(s)