Influence of microscopic defects on optical damage resistance of Zn:Fe:LiNbO3 crystals

  • 1. Department of Chemistry, Tsinghua University, Beijing 100084 (China)
  • 2. Department of Applied Chemistry, Harbin Institute of Technology, Harbin 150001 (China)

Description

Influence of defect structure on the infrared transmission spectra of OH- in Zn:Fe:LiNbO3 crystals with various ZnO concentration and different Li/Nb ratios was investigated. It indicates that above the Zn concentration threshold the OH- absorptions bands successively shift from 3482cm-1 to 3504cm-1 and 3529cm-1. The intensity of the 3504cm-1 band increases with ZnO concentration increasing. The optical damage resistance of the Zn:Fe:LiNbO3 crystals increases rapidly when the ZnO concentration exceeds a threshold value. This result contributed to the site alteration from the Li sites to Nb sites due to Zn-doping in crystal. copyright 2006 WILEY-VCH Verlag GmbH and Co. KGaA, Weinheim. (orig.)

Availability note (English)

Available from: http://dx.doi.org/10.1002/crat.200510573

Additional details

Identifiers

Publishing Information

Journal Title
Crystal Research and Technology
Journal Volume
41
Journal Issue
3
Journal Page Range
p. 276-279
ISSN
0232-1300
CODEN
CRTEDF

Optional Information

Notes
1 fig., 1 tab., 21 refs.. SICI: 0232-1300(200603)41:3<276::AID-CRAT200510573>3.0.TX;2-G