Published August 1987
| Version v1
Journal article
Effect of thickness of intermediate layers of O8Yu steel on the properties of 16GS+08Kh18N10T bimetal
Creators
- 1. Tsentral'nyj Nauchno-Issledovatel'skij Inst. Chernoj Metallurgii, Moscow (USSR)
Description
Consideration Is being given to peculiarities of formation and properties of joints of 16GS + 08Kh18N10T tYpe with soft interlayer of 08Yu steel of different thickness, produced by vacuum pressure welding and roll welding. It is shown that thickness of interlayer, providing production of joints with high strength and ductility, must lie within the range of 250-450 μm
Additional details
Additional titles
- Original title (Russian)
- Влияние толщины промежуточных прослоек из стали 08Yu на свойства биметалла 16GS+08Kh18N10T
Publishing Information
- Journal Title
- Avtom. Svarka
- Journal Issue
- no.8
- Series
- Avtom. Svarka.
- ISSN
- 0005-111X
- CODEN
- AVSVA
INIS
- Country of Publication
- Ukraine
- Country of Input or Organization
- USSR
- INIS RN
- 19044149
- Subject category
- S36: MATERIALS SCIENCE;
- Descriptors DEI
- BIMETALS; CARBON STEELS; FRACTURES; LOW ALLOY STEELS; MICROSTRUCTURE; S-N DIAGRAM; STEEL-CR18NI10TI; TENSILE PROPERTIES; THICKNESS; VACUUM WELDING; WELDED JOINTS
- Descriptors DEC
- ALLOYS; AUSTENITIC STEELS; CARBON ADDITIONS; CHROMIUM ALLOYS; CHROMIUM-NICKEL STEELS; CORROSION RESISTANT ALLOYS; CRYSTAL STRUCTURE; DIAGRAMS; DIMENSIONS; FABRICATION; FAILURES; HEAT RESISTING ALLOYS; HIGH ALLOY STEELS; INFORMATION; IRON ALLOYS; IRON BASE ALLOYS; JOINING; JOINTS; MECHANICAL PROPERTIES; NICKEL ALLOYS; STAINLESS STEELS; STEELS; TITANIUM ADDITIONS; WELDING