Description

This patent describes a method for producing films of superconductor materials. It comprises: forming a solution from the neodecanoates of europium, barium, and copper metals, the metals form an oxide mixture exhibiting superconductive properties, the solution comprises a solvent having at least approximately 10 volume percent pyridine in xylene; depositing a film of the solution onto a substrate, the substrate selected from the group consisting of strontium titanate, barium titanate, and sapphire; pyrolyzing the film in an oxygen-containing environment at a first temperature of approximately 500 degrees C. for up to approximately 5 minutes and heating the oxide film at a second temperature ranging between about 850 degrees C. and 1000 degrees C. for a duration of up to approximately 2 minutes

Availability note (English)

Patent and Trademark Office, Box 9, Washington, DC 20232 (USA).

Additional details

Publishing Information

Imprint Pagination
vp.
IPC:
Int. Cl. B05D 3/02.
IPC
Int. Cl. B05D 3/02.
Patent number
US patent document 4918051/A/

INIS

Country of Publication
United States
Country of Input or Organization
United States
INIS RN
21086135
Subject category
S36: MATERIALS SCIENCE;
Resource subtype / Literary indicator
Non-conventional Literature
Descriptors DEI
ANNEALING; BARIUM OXIDES; COPPER OXIDES; DEPOSITION; EUROPIUM OXIDES; PYROLYSIS; SUPERCONDUCTORS
Descriptors DEC
ALKALINE EARTH METAL COMPOUNDS; BARIUM COMPOUNDS; CHALCOGENIDES; CHEMICAL REACTIONS; COPPER COMPOUNDS; DECOMPOSITION; EUROPIUM COMPOUNDS; HEAT TREATMENTS; OXIDES; OXYGEN COMPOUNDS; RARE EARTH COMPOUNDS; TRANSITION ELEMENT COMPOUNDS