Published April 2000 | Version v1
Journal article

In situ purification, alloying and casting methodology for metallic plutonium

Description

The methodology for obtaining metallic plutonium through double electro-refinement with subsequent purification by zone melting is described. The content of 19 elements proved in the course of the above purification to be below the determined concentration. The metal, purified by the zone melting, was subjected to distillation through the method of the melt levitation. Gallium was introduced for the δ phase stabilization. The samples of conic form 1 cm long were obtained by melting in a water-cooled ceramic chill mold. The samples structure is characterized by grains of needle-form morphology 10 x 25 μm in size and their density equaled 15.938 ± 0.002 g/cm3

Abstract (Russian)

Описана методика получения металлического плутония путем двойного электрорафинирования с последующей очисткой зонной плавкой. В результате проведенной очистки содержание 19 элементов оказалось ниже минимальной определяемой концентрации. Рафинированный зонной плавкой металл был подвергнут дистилляции методом левитации расплава. Для стабилизации δ-фазы плутония вводили галлий. Образцы конической формы длиной 1 см получали литьем в водоохлаждаемый керамический кокиль. Структура образцов характеризуется зернами иглообразной морфологии размером 10 х 25 мкм, плотность составила 15,938 ± 0,002 г/см3

Additional details

Additional titles

Original title (Russian)
Методика рафинирования, плавки и литья металлического плутония

Publishing Information

Journal Title
Atomnaya Tekhnika za Rubezhom
Journal Issue
no.4
Journal Page Range
p. 19-23
ISSN
0320-9326
CODEN
ATRUA8

Optional Information

Notes
13 refs., 2 figs., 1 tab.