2:17 type SmCo magnets with low temperature coefficients of remanence and coercivity
Creators
- 1. Zhejiang Province Key Laboratory of Magnetic Materials and Application Technology, Ningbo Institute of Material Technology and Engineering, Chinese Academy of Sciences, Ningbo 315201 (China)
- 2. CAS Key Laboratory of Magnetic Materials and Devices, Ningbo Institute of Material Technology and Engineering, Chinese Academy of Sciences, Ningbo 315201 (China)
Description
Spin-reorientation-transition cell boundary phases are used to improve the temperature stability of coercivity in 2:17 type SmCo magnets. A magnet with both low temperature coefficients of remanence (α) and coercivity (β) is developed. In comparison with traditional 2:17 type SmCo magnets with low temperature coefficient of remanence, this magnet exhibits comparable (BH)max and α, meanwhile the β(20–100 °C) is improved by more than two orders of magnitude. The comparative study of reversible magnetization/irreversible magnetizations indicates that the flux losses of this magnet are barely affected by temperature, which is an remarkable improvement in developing temperature-stable magnet.
Additional details
Identifiers
- DOI
- 10.1016/j.jmmm.2018.10.113;
- PII
- S0304885317339902;
Publishing Information
- Journal Title
- Journal of Magnetism and Magnetic Materials
- Journal Volume
- 473
- Journal Page Range
- p. 376-380
- ISSN
- 0304-8853
- CODEN
- JMMMDC
INIS
- Country of Publication
- Netherlands
- Country of Input or Organization
- International Atomic Energy Agency (IAEA)
- INIS RN
- 55023375
- Subject category
- S36: MATERIALS SCIENCE;
- Descriptors DEI
- COERCIVE FORCE; MAGNETIZATION; MAGNETS; SPIN; TEMPERATURE COEFFICIENT
- Descriptors DEC
- ANGULAR MOMENTUM; EQUIPMENT; PARTICLE PROPERTIES; REACTIVITY COEFFICIENTS
Optional Information
- Copyright
- Copyright (c) 2018 Elsevier B.V. All rights reserved.