The effects of temperature on HEPA filter media
Description
This paper presents the results from a series of experiments to study the changes in the physical properties of HEPA filter media after exposure to elevated temperatures. Data are presented for papers heated in the range 120-500 degrees C. The observed changes in strength and paper stiffness are explained in terms of alterations to the binder due to thermal degradation. The information generated has clarified a particular failure mode associated with a small number of filter inserts at elevated temperatures
Additional details
Publishing Information
- Imprint Title
- Proceedings of the 22nd DOE/NRC Nuclear Air Cleaning Conference, Sessions 1--8
- Imprint Pagination
- 483 p.
- Journal Page Range
- p. 327-335.
- Report number
- NUREG/CP--0130-Vol.1
Conference
- Title
- 22. Department of Energy (DOE)/Nuclear Regulatory Commission (NRC) nuclear air cleaning and treatment conference.
- Dates
- 24-27 Aug 1992.
- Place
- Denver, CO (United States).
INIS
- Country of Publication
- United States
- Country of Input or Organization
- United States
- INIS RN
- 25014667
- Subject category
- S61: RADIATION PROTECTION AND DOSIMETRY; S61: RADIATION PROTECTION AND DOSIMETRY;
- Resource subtype / Literary indicator
- Conference
- Descriptors DEI
- AIR FILTERS; PHYSICAL PROPERTIES; TEMPERATURE RANGE 0273-0400 K; TEMPERATURE RANGE 0400-1000 K; THERMAL DEGRADATION; THERMAL TESTING
- Descriptors DEC
- EQUIPMENT; FILTERS; MATERIALS TESTING; NONDESTRUCTIVE TESTING; POLLUTION CONTROL EQUIPMENT; TEMPERATURE RANGE; TESTING
Optional Information
- Secondary number(s)
- CONF-920823--Vol.1.