Published July 14, 1995 | Version v1
Patent

UO2 pellet and manufacturing method

Description

The present invention concerns an uranium dioxide pellet having a large crystal grain size. The grain size of the pellet is enlarged to increase the distance of an FP gas generated in the crystal grain to reach the grain boundary and, as a result, decrease the releasing speed of the FP gas. A UO2 powder having a specific surface area of from 5 to 50m2/g is used as a starting powder in a step of forming a molding product, and chlorine or a chlorine compound is added in such an amount that the chlorine content in the UO2 pellet is from 3 to 25ppm, in one of a production step, a molding step or a sintering step for UO2 powder. With such procedures, a UO2 pellet having a large crystal grain size can be prepared with good reproducibility. (T.M.)

Availability note (English)

Available from JAPIO. Also available from EPO.

Additional details

Publishing Information

Imprint Pagination
7 p.
IPC:
Int. Cl. G21C3/62; C01G43/025.
IPC
Int. Cl. G21C3/62; C01G43/025.
Patent number
JP patent document 7-174879/A/

Optional Information

Secondary number(s)
JP patent application 5-320769.