Published June 1978 | Version v1
Report Open

Leaching of Al2O3 in simulated repository conditions

  • 1. Aktiebolaget Atomenergi, Studsvik (Sweden)

Description

Al2O3 material has been leached at 90 deg C in: simulated ground water at pH 8.5, embedded in bentonite + silica sand saturated with the same water, and in simulated ground water at pH 6 and pH 10. Leaching periods varied from 30 days to 300 days. We observed slight weight increments in all cases from deposits on samples from the environment. These mask weight losses from Al2O3 that may have occurred. (author)

Availability note (English)

MF available from INIS under the Report Number.

Files

10438333.pdf

Files (431.1 kB)

Name Size Download all
md5:6cae03dec1f5725561f63751bb980a2b
431.1 kB Preview Download

Additional details

Additional titles

Original title (Swedish)
Lakning av Al

Publishing Information

Imprint Pagination
15 p.
Report number
KBS-TR--116

Optional Information

Secondary number(s)
STUDSVIK-MS--78/213.