Effect of nickel plating upon tensile tests of uranium--0.75 titanium alloy
Description
Electrolytic-nickel-plated specimens of uranium-0.75 wt percent titanium alloy were tested in air at 20 and 100 percent relative humidities. Tensile-test ductility values were lowered by a high humidity and also by nickel plating alone. Baking the nickel-plated specimens did not eliminate the ductility degradation. Embrittlement because of nickel plating was also evident in tensile tests at -340C. (U.S.)
Availability note (English)
MF available from INIS under the Report Number.
Files
Additional details
Publishing Information
- Imprint Pagination
- 9 p.
- Report number
- Y--1987
INIS
- Country of Publication
- United States
- Country of Input or Organization
- United States
- INIS RN
- 6212756
- Subject category
- S36: MATERIALS SCIENCE;
- Descriptors DEI
- AIR; DILUTE ALLOYS; DUCTILITY; ELECTROPLATING; EMBRITTLEMENT; HUMIDITY; LOW TEMPERATURE; NICKEL; TENSILE PROPERTIES; TITANIUM ADDITIONS; URANIUM BASE ALLOYS
- Descriptors DEC
- ACTINIDE ALLOYS; ALLOYS; DEPOSITION; ELECTRODEPOSITION; ELECTROLYSIS; ELEMENTS; FLUIDS; GASES; MECHANICAL PROPERTIES; METALS; PLATING; SURFACE COATING; TRANSITION ELEMENTS; URANIUM ALLOYS