Fracture peculiarities of heat resisting Cr-Mo-V steels under creep

Description

Structural peculiarities of damages, developing under creep in (0.4-0.6)Tmel. range were investigated for samples of steam pipes of 12Kh1MF and 15Kh1M1F steels. It was established that fracture under mentioned conditions occurred when the average pore size in the fracture achieved 3±1.4 μm and the density of pore distribution was equal to 0.03-0.06 μm-2. These parameters are independent of chemical composition and structure of steels

Additional details

Additional titles

Original title (Russian)
Исследование особенностей разрушения при ползучести теплостойких Cр-Мо-В-сталей