[en] Temperature dependencies of pyrocoefficient for a wide class of various pyroactive crystals in the temperature range from 4,2 to 300 deg K were investigated. The problems to be solved were: to confirm a conclusion on the pyrocoefficient γsup(sigma) tending to zero at T → 0; to compare experimental data with conclusions of existing theories; to reveal specific features in the behaviour of both linear pyroelectrics and segnetoelectrics at low temperatures. The behaviour of the total pyrocoefficient for all crystals obeys the regularity γsup(sigma) → 0 at T → O. In the range of low temperatures the pyrocoefficient varies by the power law: γsup(sigma) approximately Tsup(α). For the majority of crystals studied α is close to 3. CdS, BeO, ZiNbO3 and other crystals were studied
Original Title
Povedenie polyarnykh kristallov pri nizkikh temperaturakh
Secondary Subject
Source
8. all-union conference on ferroelectricity; Uzhgorod, Ukrainian SSR; 1 Sep 1974; For English translation see the journal Bull. Acad. Sci. USSR, Phys. Sci.
Record Type
Journal Article
Literature Type
Conference
Journal
Izvestiya Akademii Nauk SSSR, Seriya Fizicheskaya; v. 39(5); p. 990-994
Country of publication
Reference NumberReference Number
INIS VolumeINIS Volume
INIS IssueINIS Issue