AbstractAbstract
[en] While transported through a tin bath, the niobium foil is covered with tin and is annealed. Excess tin is removed from the annealed foil and the foil is re-annealed at a temperature of 900 to 970 degC for over 5 to 30 mins. Thus, a significant increase is achieved in critical current. (J.P.)
Original Title
Sposob vyroby supravodivych pasok
Source
15 Sep 1981; 2 p; CS PATENT DOCUMENT 190009/B/
Record Type
Patent