Filters
Results 1 - 1 of 1
Results 1 - 1 of 1.
Search took: 0.014 seconds
Maile, K.; Theofel, H.; Buehrer, S.
17th colloquium on long-time behaviour of heat-resistant steels and high-temperature materials1994
17th colloquium on long-time behaviour of heat-resistant steels and high-temperature materials1994
AbstractAbstract
[en] At present structure casts represent the only non-destructive method by which it is possible to recognise creep damage early. For this reason, the possibilities of quantification and the description of the individual damage behaviour of the materials 10 CrMo 9 10 and X 20 CrMo V 12 1 are dealt with here by metallographic examination. (orig./MM)
[de]
Zur Zeit stellen Gefuegeabdruecke die einzige zerstoerungsfreie Methode dar, mit der es moeglich ist, Kriechschaedigungen fruehzeitig zu erkennen. Aus diesem Grund soll hier auf die Moeglichkeiten der Quantifizierung und der Beschreibung des individuellen Schaedigungsverhaltens der Werkstoffe 10 CrMo 9 10 und X 20 CrMo V 12 1 anhand von metallografischen Untersuchungen eingegangen werden. (orig./MM)Original Title
Ermittlung und Beschreibung der Schaedigung in langzeitbelasteten Zeitstandproben
Primary Subject
Source
Verein Deutscher Eisenhuettenleute (VDEh), Duesseldorf (Germany); 196 p; 1994; p. 173-183; Colloqium on long-time behavior of heat-resistant steels and high-temperature materials; Kolloquium ueber Langzeitverhalten Warmfester Staehle und Hochtemperaturwerkstoffe; Duesseldorf (Germany); 25 Nov 1994; Available from TIB Hannover: RO 1809(17)
Record Type
Miscellaneous
Literature Type
Conference
Country of publication
Reference NumberReference Number
INIS VolumeINIS Volume
INIS IssueINIS Issue