AbstractAbstract
[en] The paper presents new experimental data on the electrical conductivity sigma and the absolute thermoelectric power S of liquid Cs-Au alloys in the concentration range 0 to 60 at% Au and at temperatures up to 7200C. It is found that near the composition CsAu the sigma-curve and the S-curve have deep minima with values of about 3 Ohm-1 cm-1 and -1,400 μV/K, respectively which are of the same order of magnitude as those of the molten salts. It is found that existing theories about 'liquid semiconductors' cannot account for the observed metal-nonmetal transition in liquid Cs-Au. Therefore as an alternative hypothesis it is proposed that in Cs-Au near the equi-atomic concentration ionic conduction plays an important role. (orig.)
[de]
Die Arbeit berichtet ueber neue Messungen der elektrischen Leitfaehigkeit sigma und der absoluten Thermokraft S von fluessigen Cs-Au-Legierungen im Konzentrationsbereich von 0 bis 60 Atom% Au bei Temperaturen bis zu 7200C. Die sigma- und S-Kurven haben tiefe Minima in der Naehe der Cs-Au-Zusammensetzung mit Werten von 3 Ohm-1 cm-1 bzw. -1.400 μV/grad, die in der Groessenordnung den Werten fuer geschmolzene Salze sehr aehnlich sind. Die Resultate koennen nicht mit den existierenden Theorien ueber 'fluessige Halbleiter' gedeutet werden. Deshalb wird eine Hypothese aufgestellt, die annimmt, dass in der Naehe der CsAu-Konzentration Ionenleitung eine wichtige Rolle spielt. (orig.)Primary Subject
Secondary Subject
Source
9 figs.; 29 refs.
Record Type
Journal Article
Journal
Berichte der Bunsengesellschaft fuer Physikalische Chemie; v. 80(2); p. 107-113
Country of publication
Reference NumberReference Number
INIS VolumeINIS Volume
INIS IssueINIS Issue